Need a brief explanation of the sulfur degassing process
 
Have you tried Google?
 
Thanks TD2K, I have tried google, just looking for other views
 
You have two degassing effects, one to remove the physically entrained H2S that exist in the tail ags and is soluble in the liquid sulphur. The other "degassing" comes from polysulphides that gets oxidised. This can be done with (cheap) air blowing it into the sulphur pit through spargers or e.g. chemically with an "catalysing" (chemical) agent, that releases the H2S.
there is a good book written by previous Wsetern research (now Global sulphur) that was the best one when I used to work on Claus/TGTU units, you find a link to them through
MainSx/SxMainPage.htm .
Try out for Shell process and for a catalytic version.
RH
 
Western Research is now part of AMETEK Process Instruments. They are a combination of the Western Research and AMETEK (formerly DuPont) instruments businesses.

I recommend that you either contact SulphurExperts ( or AMETEK Process Instruments ( or
You may also want to consider monitoring the liquid sulfur's head space for SO2 and H2S concentrations. They are a useful indication of hazardous conditions within the liquid storage or degassing tank. For example, an elevated SO2 concentration in the vapor space above liquid sulfur can indicate the presence of a smoldering sulfur fire.
 
I can recommend another company ... CBI TPA.
They have extensive experience in this field and they are an industry leader in the design of Sulfur Recovery Units.

Typically we use a mechanical agitation and sweep process or a licensed catalyst process, which our process engineers will be glad to explain to you.
 