Feb 23, 2006 #1 UTChemE Chemical Joined Dec 19, 2004 Messages 8 Location US Greetings all Does anybody know of a sulfur inhibitor that will not interfere with in-situ leaching of uranium? Wells need to be periodically cleaned and acidized, this cuts down on production time, etc. Thanks. Blessings.
Greetings all Does anybody know of a sulfur inhibitor that will not interfere with in-situ leaching of uranium? Wells need to be periodically cleaned and acidized, this cuts down on production time, etc. Thanks. Blessings.
Apr 3, 2006 #2 EdStainless Materials Joined May 20, 2004 Messages 16,399 Location Waukesha WI USA What compounds are actually forming? Is it pure sulfur or sulfides? Any other mineral scales forming? = = = = = = = = = = = = = = = = = = = = Rust never sleeps Neither should your protection http://www.trent-tube.com/contact/Tech_Assist.cfm Upvote 0 Downvote
What compounds are actually forming? Is it pure sulfur or sulfides? Any other mineral scales forming? = = = = = = = = = = = = = = = = = = = = Rust never sleeps Neither should your protection http://www.trent-tube.com/contact/Tech_Assist.cfm