May 23, 2007 #1 mikeo56 Structural Joined Jun 3, 2003 Messages 28 Location US I am looking for an adhesive that is suitable for attaching 3/8" thick granite to the face of a stainless fireplace.
I am looking for an adhesive that is suitable for attaching 3/8" thick granite to the face of a stainless fireplace.
May 25, 2007 #2 sreid Electrical Joined Mar 5, 2004 Messages 2,127 Location US Locktite is advertizing Sumo Glue. http://www.sumoglue.com/ Upvote 0 Downvote
May 25, 2007 #3 Compositepro Chemical Joined Oct 22, 2003 Messages 7,841 Location US RTV Silicone would probably be your best choice. Apply it in spots about 1/8" thick by 1" in diameter. You can use two sided pressure sensitive tape (like 3M VHB) to fixture things in place until the silicone cures enough (at least 24 hours). Upvote 0 Downvote
RTV Silicone would probably be your best choice. Apply it in spots about 1/8" thick by 1" in diameter. You can use two sided pressure sensitive tape (like 3M VHB) to fixture things in place until the silicone cures enough (at least 24 hours).