Hello all,
I work in an operating company in which I came across the below criteria for stainless steel:
Stainless steel may be used in offshore applications up to an operating temperature of 60 degC.
As per my understanding, the above temperature limitation governs in case of sour service and a chloride content of 50ppm as per NACE MR0175/ISO 15156.
Appreciate your opinions on this matter.
I work in an operating company in which I came across the below criteria for stainless steel:
Stainless steel may be used in offshore applications up to an operating temperature of 60 degC.
As per my understanding, the above temperature limitation governs in case of sour service and a chloride content of 50ppm as per NACE MR0175/ISO 15156.
Appreciate your opinions on this matter.