balven
Materials
- Aug 29, 2011
- 9
In one of our projects we are designing a Sour Water Stripping Unit with a Sour Water Stripper Column and a pump-around loop (on the top section of Stripper Column) which has a pump, an air cooler and associated piping. The top section of the Stripper Column is specified as clad with SS316L, the pump in the loop is also SS316, while the air cooler and pump-around piping is 22Cr Duplex Stainless Steel (DSS). Process conditions in this pump-around loop are as follows :
Temperature : Top section of Stripper column is maintained at 90 deg. C. The pump takes sour water at 96 deg. C and sends it to the air cooler which cools it down to 60 deg. C before returning the sour water to the Column.
Pressure : 8 bara maximum
Fluid Composition : H2S : 5.1 wt%, NH3 : 8.43 wt%; expected ammonium bisulphide : around 7.5 wt%; chlorides : 10 ppmw; CO2 : 0.02 wt%
No cyanides are expected to be present.
Fluid velocity : 2 m/s maximum
Based on the above process conditions, is it OK to use SS316 / DSS for this pump-around section ? If not, up to what level should the ammonium bisulphide concentration be brought down to (such as by water washing) in order for SS316 / DSS to be suitable for the above temperatures, pressure and fluid velocity ? Any opinions / past experiences / references will be much appreciated.
Thanks
Balvendra Pal
Temperature : Top section of Stripper column is maintained at 90 deg. C. The pump takes sour water at 96 deg. C and sends it to the air cooler which cools it down to 60 deg. C before returning the sour water to the Column.
Pressure : 8 bara maximum
Fluid Composition : H2S : 5.1 wt%, NH3 : 8.43 wt%; expected ammonium bisulphide : around 7.5 wt%; chlorides : 10 ppmw; CO2 : 0.02 wt%
No cyanides are expected to be present.
Fluid velocity : 2 m/s maximum
Based on the above process conditions, is it OK to use SS316 / DSS for this pump-around section ? If not, up to what level should the ammonium bisulphide concentration be brought down to (such as by water washing) in order for SS316 / DSS to be suitable for the above temperatures, pressure and fluid velocity ? Any opinions / past experiences / references will be much appreciated.
Thanks