Good day Gentlemen,
I need some help selecting a grade of hot work steel or other variety that will survive in this environment.
Application- Nozzle for extruding abrasive plastics at high temperatures. Nozzle measures 3mm long X 1.5mm in diameter with a through hole starting at .75mm then stepping down to .25mm.
Requirements-
-maintain properties up to 450c
-good abrasion resistance
-fair machinability
-fair ductility, pre hardened (cold forming of tip may be required to reduce orifice size)
-corrosion resistant
-commonly available
Nozzle will not experience any physical abuse in service. Thanks in advance
I need some help selecting a grade of hot work steel or other variety that will survive in this environment.
Application- Nozzle for extruding abrasive plastics at high temperatures. Nozzle measures 3mm long X 1.5mm in diameter with a through hole starting at .75mm then stepping down to .25mm.
Requirements-
-maintain properties up to 450c
-good abrasion resistance
-fair machinability
-fair ductility, pre hardened (cold forming of tip may be required to reduce orifice size)
-corrosion resistant
-commonly available
Nozzle will not experience any physical abuse in service. Thanks in advance