Hello all,

I'm a new member of this group.. I have few questions. i work for a hydrometallurgy company and was wondering if any can help me.

Questions..

we extract metal which has mn and Fe and zn.. is there
any good membrane which removes mn and Zn by electrolysis or is there any resin which would remove both of these metals

Thank u experts