Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations dmapguru on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Suggestion: Laser Welding System for Thin Stainless Steel & Non-Linear Weld Paths?

Status
Not open for further replies.

Helepolis

Mechanical
Joined
Dec 13, 2015
Messages
214
Location
IL
Hi all,

Just to clarify that at the moment I'm just exploring the options in general, to see if there is any viability in this at all.

At my workplace there is a need to weld thin pieces of sheet metal (0.2-0.5mm thickness; CRES 321, CRES 347) along a non-linear weld-path.
At the moment the work is done by hand, and I was wondering if there is an "affordable" (lets say ~80-150K$) laser welding machine semi or fully automated which can handle thin metal parts and non-linear weld paths.

I have googled a bit to see what can I find, but since I have never dealt with such devices I have no idea which machine is good, reliable etc...


Thanks,
SD
 
They are out there. I have seen them, but not familiar with brands. It also depends how large your parts are.
Pick some in your Google search and have them do a demo for you.
 
"non-linear"........describe and specify precisely, including required path accuracy and acceptable tolerances. There is a lot of difference between simple arc paths in a plane and complex 3D swoopy-curvy paths
"affordable ~80-150K$".......this may not be a sufficient budget for a complex path with high tolerance requirements
Should it be assumed your welding process is fully developed and characterized (wavelength, pulsed vs full-wave, power levels, etc)?

As a former robotics guy, I can envision an "affordable" solution with a 6-axis robot for swoopy-curvy 3D paths. But that would depend upon your programming resources, path specification, process quality requirements, and production requirements.
 