Dear Colleagues,
I have a problem by understanding the following:
The granular Subbase is supposed to be a lower quality material than the granular base.
If I refer to the "1993 AASHTO Guide for Design of Pavement Structures" to obtain the layer coefficients, I get the following:
a) Layer coefficient a2 for a granular base with CBR 30% is 0.095 (Part II, Table 2.6)
b) Layer coefficient a3 for a granular Subbase with CBR 30% is 0.11 (Part II, Table 2.7).
Hence a granular Subbase with same thickness and same CBR would create a higher SN than a granular Base though it is in general "lower quality".
What have I missed ???
Thank you,
MARTIN
I have a problem by understanding the following:
The granular Subbase is supposed to be a lower quality material than the granular base.
If I refer to the "1993 AASHTO Guide for Design of Pavement Structures" to obtain the layer coefficients, I get the following:
a) Layer coefficient a2 for a granular base with CBR 30% is 0.095 (Part II, Table 2.6)
b) Layer coefficient a3 for a granular Subbase with CBR 30% is 0.11 (Part II, Table 2.7).
Hence a granular Subbase with same thickness and same CBR would create a higher SN than a granular Base though it is in general "lower quality".
What have I missed ???
Thank you,
MARTIN