bulldog2002
Structural
I am trying to qualify Welding Procedures to AWS D1.1. My base metal has a CVN impact toughness of 430j @-50c, testing labs are not willing to test fill size CVN samples at this strength, they will only test subsized samples.
AWS D1.1, clause 4, paragraph 4.36.5 stats that no subsized CVN samples may be used if base material is over 11mm (ours is between 15mm and 30mm).
Also in D1.1, clause 4, paragraph 4.37.1 states that if my base metal yield strength is above 50ksi (ours is approx 52ksi and above) then the contractor documents shall specify CVN testing requirements. None of our customers specify anything but testing temperature and min results required.
Does anyone know of any paragraphs or verbiage that would allow me to do PQR's to D1.1 and use subsized samples?
AWS D1.1, clause 4, paragraph 4.36.5 stats that no subsized CVN samples may be used if base material is over 11mm (ours is between 15mm and 30mm).
Also in D1.1, clause 4, paragraph 4.37.1 states that if my base metal yield strength is above 50ksi (ours is approx 52ksi and above) then the contractor documents shall specify CVN testing requirements. None of our customers specify anything but testing temperature and min results required.
Does anyone know of any paragraphs or verbiage that would allow me to do PQR's to D1.1 and use subsized samples?