pgsturbine
Mechanical
- May 3, 2006
- 2
Project involves a 1 1/2" x 8tpi steam turbine stud and its fitment to the internal threads of the turbine casing horizontal joint flange. In defining the acceptability of the internal flange studs we would be looking to insert the stud into the flange a distance of 1 times the thread diameter. We would look to indicate the movement of the stud by dial indicator method. We anticipate that the acceptance criteria would be something less that .008" movement. The question would be at what distance from the flange would the indication of the stud movement be taken?