Does ASME Sec VIII-Div 1, said about acceptance criteria for visual weld inspection of stud welds?
Any reference?
Thanks in advance.
BPVN
 
Replies continue below

Recommended for you

No criteria for visual inspection because a visual inspection is not going to be effective. I would conduct a rake test and see how many studs remain.
 