Jun 29, 2004 #1 Gadgetmark Mechanical Joined Jun 28, 2004 Messages 2 Location AU Can anyone give me dimensions, particularly of the curved shape (torispherical?), for a 250NB, SCH40S, ASTM A403 316L Stainless Steel End Cap?
Can anyone give me dimensions, particularly of the curved shape (torispherical?), for a 250NB, SCH40S, ASTM A403 316L Stainless Steel End Cap?
Jul 2, 2004 #2 arto Mechanical Joined Jun 19, 2002 Messages 712 Location US Try these guys - their catalog is like the old Ladish ones: http://www.weldbend.com/tableofcontents.htm Upvote 0 Downvote
Try these guys - their catalog is like the old Ladish ones: http://www.weldbend.com/tableofcontents.htm