Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Structural Shapes 3

Status
Not open for further replies.

Acoona

Structural
Feb 4, 2004
3
I am beginning to review some existing steel and am having trouble finding properties on some of them. I cannot find 14B17.2, 7I15.3??
Does anyone nkow where I can find info on these mebemer sizes? The drawings are dated in the mid 1960's if that helps,
Thanks in advance,
 
Replies continue below

Recommended for you

The second is now called a S7 x 15.3 and is commonly called a standard shape. It's still in any AISC Manual.
I can't figure out the first one.
 
According to the AISC database under ASD6, the first one may have been called B14x4.

w=17.2
A=5.05
d=14.00
tw=0.21
bf=4.00
tf=0.272
Ix=147.3
Iy=2.65
 