Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations dmapguru on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Structural Modelling of Wire Ropes

Status
Not open for further replies.

SewardWyon

Mechanical
Joined
Apr 6, 2009
Messages
3
Location
GB
We have just acquired a copy of SCIA Engineer 2008.1 structural analysis and FEA software, and I am the primary user of this software. I am designing a flare boom for mounting on deep sea drilling ships. It is a lattice structure, triangular in section, is hinged at the root where it connects to the ship and supported by guy wires anchored 15m above the boom root and attaching to 2 points approxiamatly 1/3 and 2/3 along its length. The problem I have is modelling the wire ropes realistically, so that the catenary and spring effects of the rope are taken into account. Both these factors could contribute to the boom resonating at its natural frequency.
Thanks in advance
 
Well, with no answers I'll take a stab.

You can either model them as tension members, and then use a linear analysis, or else you'll have to do a non linear analysis in which case your 'resonant frequencies' will change with excitation amplitude. That is a pain.

If you can assume that the wires stay in tension all the time, and that their self resonances are unimportant, then the linear approach should work.




Cheers

Greg Locock