Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Stripping Mineral Insulated Cable

Status
Not open for further replies.

rk215

Mechanical
Joined
Aug 9, 2002
Messages
3
Location
US
Does anyone know of any durable tooling for stripping Mineral Insulated Cable
 
What you need is a Cable Stripper for stripping MICC/MIMS/PYRO (or whatever you want to call it)
Available from all good electrical wholesalers or companies like RS.
I made my own by welding some 8mm bar into a "T" shape then slotting the end with a hacksaw for about 15mm.
It takes a bit of practice but with a pipe cutter to score the sheath and some side cutter snips it works OK, and can strip any diameter without adjustment. "I love deadlines. I love the whooshing noise they make as they go past." Douglas Adams
 