Perhaps a stupid question, but here I go....
How do I input stress/strain data from a tensile test into an elasto-plastic material model in FEA?
The program states that the starting point should be the yield point.
Attached You'll find the results and graphs from 2 tests bars.
Result on testbar 215:
Rp0,2: 182 MPa
Rm: 229,1 MPa
At: 0,927
The data file, and plotted curve, shows 120 MPa at 0,2% strain.
So in the results file, the initial slope (E modulus) is parallel moved to 0,2% to hit the curve at 182 MPa.
How do I handle this in my FEA program material model to capture the elasto plastic behaviour?
Should i modify all the strain values so 182 MPa corresponds to 0,2%, instead of about 0,5% for the moment or should my start point be 182/0,5?
Thank you in advance for your help.
Perhaps a stupid question, but here I go....
How do I input stress/strain data from a tensile test into an elasto-plastic material model in FEA?
The program states that the starting point should be the yield point.
Attached You'll find the results and graphs from 2 tests bars.
Result on testbar 215:
Rp0,2: 182 MPa
Rm: 229,1 MPa
At: 0,927
The data file, and plotted curve, shows 120 MPa at 0,2% strain.
So in the results file, the initial slope (E modulus) is parallel moved to 0,2% to hit the curve at 182 MPa.
How do I handle this in my FEA program material model to capture the elasto plastic behaviour?
Should i modify all the strain values so 182 MPa corresponds to 0,2%, instead of about 0,5% for the moment or should my start point be 182/0,5?
Thank you in advance for your help.