I am having some trouble finding info on stress relieving high carbon material? I have 1050-1055 Rb 84 min. stock. What temperature is best to take out any stresses?
 
Replies continue below

Recommended for you

Stress relief at 1100-1150 deg F for 1 hour per inch of thickness will work.
 