Kurniatullah
Mechanical
Dear Professional,
Now, i preparing procedure for heat treatment,
i have equipment as below condition
- Material SA516-70N
- Extreme Fiber elongation over than 5%
- PWHT should be performed due to special service,
my question: whether we can performed PWHT only, due to stress relieve will cover by PWHT.
please inform applicable code to be used.
please advice,
Regards
KRN
Now, i preparing procedure for heat treatment,
i have equipment as below condition
- Material SA516-70N
- Extreme Fiber elongation over than 5%
- PWHT should be performed due to special service,
my question: whether we can performed PWHT only, due to stress relieve will cover by PWHT.
please inform applicable code to be used.
please advice,
Regards
KRN