I need to know at what temp. to stress relieve 347 stainless steel.
 
Replies continue below

Recommended for you

for our stainless we use 475F for an hour or so....


ncik
 
Opinions vary but from my experience you may want to try 1625-1650F to PWHT or thermally stabilze 347 SS.
 