stress relief

Status
Not open for further replies.

engineer54

Mechanical
Jul 14, 2013
26
Can a 2 piece head welded with a stress relieve weld procedure be welded to a vessel with a non stress weld procedure?
Vessel will not be stress relieved.
 
Replies continue below

Recommended for you

Yes, as long as the head was stress relieved.
 