Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Stress Ratio & Impact testing

Status
Not open for further replies.

Corgas

Materials
Dec 22, 2008
115
Colleagues,

After calculating stress ratio according to ASME B31.3 (2008 edt) Fig. 323.2.2B, General note (a)(1), number is well below 0.3 (it doesn't intersect curve). What reduction in minimum design temperature can I use?

Thanks in advance.

Corgas
 
Replies continue below

Recommended for you

See table 323.2.2 and read all of the notes on the next page, especially note 3.

I don't think you need to use figure 323.2.2(b) for anything but the definition of what the stress ratio is.

- Steve Perry
This post is designed to provide accurate and authoritative information in regard to the subject matter covered. It is offered with the understanding that the author is not engaged in rendering engineering or other professional service. If you need help, get help, and PAY FOR IT.
 
For carbon steels, I think you impact test below -55 F (-48 C) irrespective of stress ratio.