Faribaaa

Student
Apr 19, 2021
2
Hi,
In a simple tube drawing model with a floating plug, I try to find the stress on the plug but I can only see the RF of the plug. I appreciate your help to solve this problem.
Plug_a293b7.jpg

The tools: die and plug are not rigid bodies.

Best regards,
Fariba
 