Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations LittleInch on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

stress decay distance for seal groove

Status
Not open for further replies.

DowneastTech

Mechanical
Joined
Feb 15, 2003
Messages
15
I have a thick wall, steel shell (cylinder) with two internal seal grooves. These grooves are stress risers. Now the literature specifies a stress decay distance of k x square root of (R x t) for various types of discontinuities. The value of k used varies from Pi/2 to Pi/4 to 1.0 to 0.5 and sometimes 1.1. How does one select the appropriate value for k ? I presume that it depends on the type of stress, but so far, I haven't been able to see a pattern. Can anyone help with this?

Best regards,
Downeast Tech

DowneastTech
Mechanical Engineer
Magnus R & D, Cypress, TX
 
The problem with the literature is that it never has exactly your case.

If you need to know, you gotta test it.
 
...or model it. Except that I wouldn't trust an unverified model, so you've got to test anyway.
 
p.s. if you have 2 O-ring grooves, be sure to vent in between so you don't get a "pressure trap" from thermal expansion etc.
 
Oddly, I would, in this case since I see no practical way of correlating in detail, other than to compare the k from the book with the k from the model.

I'm assuming this is a fatigue problem, not statics.



Cheers

Greg Locock