I am working at an oil refining company and considering about stress analysis on piping.
Could some explain to me how will I do about gap(1ea,20mm)between pipe line supports and structure after operating.
?Operating Temperature : 600’c
Operating Pressure : 26kg/cm2
?Piping Material : TP321
?Piping Size : 20”
Is it possible to operate it to keep remaining gap?
Could some explain to me how will I do about gap(1ea,20mm)between pipe line supports and structure after operating.
?Operating Temperature : 600’c
Operating Pressure : 26kg/cm2
?Piping Material : TP321
?Piping Size : 20”
Is it possible to operate it to keep remaining gap?