From a corrosion POV, I really despise intermittent welds.
Also from a corrosion POV, for a bolted cover plate I would be sure to finish all drilling/cutting operations, round sharp edges, degrease, prime everything but the bolts with a good epoxy zinc primer, then assemble with galvanized bolts.
Touch up the primer and finish applying your paint system after the bolting.