Hi All,
Where do you find Fy and Fu of A992 or A36?

Thanks,
 
I have not AISC 13 but the LRFD 1993 code had a table 2 within the code. Or make some google search (sounds irregular but may be effective). For A36 liste 36 ksi=Fy and Fu ranges from 58 to 80 ksi.

A992 I don't have at first sight but let's see google...

great, AISC's values

 
AISC Manual locations:

13th - Table 2-3, page 2-39
LRFD 3rd - Table 2-1, page 2-24

A-992 was not a spec before these two manuals were printed, so it does not appear in any manual prior to these.