strength of steels at elevated temperature

Status
Not open for further replies.

weissman530

Mechanical
Joined
Jun 11, 2001
Messages
4
Location
US
Can somebody direct me to a source of strength of materials data for elevated temperatures in the 600 deg F and above range?
 
THe ASME Boiler and Pressure Vessel Code, Section II provides allowable stresses for many grades of materials at elevated temps. The criteria used for stress determination is also provided. So, you many be able to "back into" some of the info you seek.

Steve Braune
Tank Industry Consultants
 
also, API std 560 has some temperature-strenght data for materials used in that area (heaters for refinery service)
 