Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Strength of cast threads

Status
Not open for further replies.

cjholl0

Automotive
Dec 15, 2006
17
Im trying to specify a torque value for a bolt that is screwed into a cast iron box. The recommended torque, using the recommended preload, is pretty straightforward from the Machinery's Handbook. But, this also assumes your using a similiar grade of nut (I think). I'm using a grade 8 bolt so I'm pretty sure the cast iron threads will break first. I don't want to torque the bolt to it's recommended value and then over stress the weaker cast threads. Is there a rule of thumb or equation that addresses this kind of situation?

Thanks
 
Replies continue below

Recommended for you

As a general rule we would use a bolt stress of 15,000-25,000 psi for all bolting when using Cast Iron.

We would try not to use high strength bolting for CI. . The fasteners were mostly ASTM A108 material.

As posted above knowing your material and with judicious application of torque you could use a higher strength fastener.
 
Here is the equation for calculating strength of tapped threads: