Dear all!
We have received very strange SDD pipe welded joint corrosion test (acc NORSOK M-601/ASTM G48) result. Weight loss is 40 g/m2, but no pitting on sample surface. Pickling (5%HF+20%HNO3) was performed before corrosion test.
Micro examination result is acceptable: no continuous precipitation and intermetallic phases.
Ferrite content is adequate too: cup 56%, root 46%, HAZ -59%, BM-50%.
Weld quality is good: no external/internal defects.
We perform about 10-15 corrosion test in week and we haven't gotten result like this.
Is it possible?
Thank you in advance!
We have received very strange SDD pipe welded joint corrosion test (acc NORSOK M-601/ASTM G48) result. Weight loss is 40 g/m2, but no pitting on sample surface. Pickling (5%HF+20%HNO3) was performed before corrosion test.
Micro examination result is acceptable: no continuous precipitation and intermetallic phases.
Ferrite content is adequate too: cup 56%, root 46%, HAZ -59%, BM-50%.
Weld quality is good: no external/internal defects.
We perform about 10-15 corrosion test in week and we haven't gotten result like this.
Is it possible?
Thank you in advance!