Hi there
hope you are fine
Please, I would like to ask you some piece of advice if possible, since I am finding some results I can't explain.
Following is the topic
I have some copper fin heat exchangers - and copper tube - in costal area, having 6 years of service
Basically the area is not industrial, therefore I would consider the solution appropriate.
Nonetheless, this is what happens
- the copper fins are very soft to touch, and seem to be falling apart soon.
- the neat heat exchanger, with vinyl fins, is not corroded !
Please any thought about this ?
Basically I would expect copper to be corroded later than aluminum, and this can't be a Cl attack, since Al would corrode before copper.
May this be a S2 or N2 attack ?
Does anybody of you know any case history ?
Many thanks
hope you are fine
Please, I would like to ask you some piece of advice if possible, since I am finding some results I can't explain.
Following is the topic
I have some copper fin heat exchangers - and copper tube - in costal area, having 6 years of service
Basically the area is not industrial, therefore I would consider the solution appropriate.
Nonetheless, this is what happens
- the copper fins are very soft to touch, and seem to be falling apart soon.
- the neat heat exchanger, with vinyl fins, is not corroded !
Please any thought about this ?
Basically I would expect copper to be corroded later than aluminum, and this can't be a Cl attack, since Al would corrode before copper.
May this be a S2 or N2 attack ?
Does anybody of you know any case history ?
Many thanks