As per A500 - Standard Specification for Cold-Formed Welded and Seamless Carbon Steel Structural Tubing in Rounds and Shapes

" 1.2 This tubing is produced in both welded and seamless sizes with a maximum periphery of 64 in. (1626 mm) and a maximum wall of 0.625 in. (15.88 mm). Grade D requires heat treatment.

11.4 Straightness—The permissible variation for straightness of structural tubing shall be 1⁄8 in. times the number of feet (10.4 mm times the number of metres) of total length divided by 5."​

1) Can I use the above formula for P22 of any other pipe i.e. ss?
2) Can anyone please differentiate structural tubing to pipe we normally use as nozzles in a vessel or drum?
3) Can anyone share a code or reference to where I can find and compute for the tolerance of pipe straightness?


thanks.
 
Each product spec has its own rules. And while you will find that many use a common wording you don't know until you check.
This spec gives you 0.125"/5 per foot, or 0.025"/ft. I know of tubular specs that are tighter (some are 0.030"/3') and some that are looser.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
You will find straightness and other general standards for alloy and SS pipe (including P22) in ASTM A999.
 
But you need to look in product specs, they don't all default to the general A999 (pipe) or A1016 (tube) specs.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 