Team,
I have a two different standerd for the strightness of bar in front of me.
Material : Brass 385
Length :3.6meter (12 ft.)
Outside diamter:56.5mm
Raw material Supplier specefication
Straightness tolerances (Ref Table 8.1:AS1567) for the specified external dimensions over 40mm up to and including 70mm straightness Tolerances (max.) in total lenght is 3.0xlength (m).
So in my case 3.0 x 3.6meter = 10.8mm.
Barfeeder supplier:
For optimum results, the bar stock must be straight. Should the bar stock exceed 0.5mm/m straightness.
Our experience says that Barfeeder supplier is right, exceeding then this cause jamming of bar.
Is any one have any clue what we is the resonable demad of strighness we have to ask from supplier.
Thanks,
R. Modi
I have a two different standerd for the strightness of bar in front of me.
Material : Brass 385
Length :3.6meter (12 ft.)
Outside diamter:56.5mm
Raw material Supplier specefication
Straightness tolerances (Ref Table 8.1:AS1567) for the specified external dimensions over 40mm up to and including 70mm straightness Tolerances (max.) in total lenght is 3.0xlength (m).
So in my case 3.0 x 3.6meter = 10.8mm.
Barfeeder supplier:
For optimum results, the bar stock must be straight. Should the bar stock exceed 0.5mm/m straightness.
Our experience says that Barfeeder supplier is right, exceeding then this cause jamming of bar.
Is any one have any clue what we is the resonable demad of strighness we have to ask from supplier.
Thanks,
R. Modi