Oct 20, 2016 #1 7mayda Petroleum Joined Feb 2, 2016 Messages 15 Location TN Hi, Can someone helps me to find/tell me where is the right procedure for the ITP(Radiography : spot, fully or 100%/Visual Inspection) of this pipeline's circumferential butt welded joints. Thanks.
Hi, Can someone helps me to find/tell me where is the right procedure for the ITP(Radiography : spot, fully or 100%/Visual Inspection) of this pipeline's circumferential butt welded joints. Thanks.
Oct 20, 2016 #2 BigInch Petroleum Joined Jun 21, 2006 Messages 15,161 Location GB The ASME B31.4 or B31.8 code has requirements for the inspection of welds stating how much must be radiographed in various. API 1104 is used as the welding standard for pipelines. Upvote 0 Downvote
The ASME B31.4 or B31.8 code has requirements for the inspection of welds stating how much must be radiographed in various. API 1104 is used as the welding standard for pipelines.
Oct 20, 2016 #3 LittleInch Petroleum Joined Mar 27, 2013 Messages 23,070 Location GB The right procedure is either as BI states or as written in the client specification. For that line I would suspect 10% RT but depends if you're the client or the contractor.... Remember - More details = better answers Also: If you get a response it's polite to respond to it. Upvote 0 Downvote
The right procedure is either as BI states or as written in the client specification. For that line I would suspect 10% RT but depends if you're the client or the contractor.... Remember - More details = better answers Also: If you get a response it's polite to respond to it.
Oct 20, 2016 #4 BigInch Petroleum Joined Jun 21, 2006 Messages 15,161 Location GB After the mobilization cost you can probably do all joints on the entire 6km for nearly the same price. I'd do them all as, for such a short pipeline like that, it probably won't ever be very far from either end facilities or civilization. Upvote 0 Downvote
After the mobilization cost you can probably do all joints on the entire 6km for nearly the same price. I'd do them all as, for such a short pipeline like that, it probably won't ever be very far from either end facilities or civilization.