Hello,

I am working with the client regarding storage tank (API 650 code)- build 1960 - 304 SS Material, ID = 14', H = 20'

Per fabrication drawing, the shell thickness was = 3/16" = 0.1875" so per specification I build the tank model in TANK software. No problem.

last month, they did the inspection at couple of places and the Ave. wall thickness is = 0.201"

My question - How come the value get higher. I thought because of the Corrosion (If any for 304 SS0,it will be lower?

Please let me know your expertise.

I appreciate your help.

Regards,
Mayur
 
The 3/16" is a "nominal" thickness. While steel is manufactured to a nominal thickness, the actual steel thickness may vary slightly. The tolerance is specified by the codes. Refer to the link for examples of the steel manufacturing tolerances.

 
The minimum shell thickness should be based upon calculations or the standard's minimum + corrosion allowance. As long as the thickness is above 3/16" the tank is still meeting the requirements of API 650 (which is a tank construction standard). A lot of tanks constructed in accordance with API 650 are operated & maintained in accordance with API 653 (which typically has a lower minimum shell thickness requirement, but does require routine inspections).
 
I appreciate your input.
Thanks - Mayur
 