Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Stock Loss Prediction

Status
Not open for further replies.

gciriani

Materials
May 5, 2004
52
In mass deburring, I try to predict the stock loss I need, by using as a proxy the material ratio curve of the surface roughness (Abbott Firestone curve), or BAC. I correlate the material loss to an approximation of the area below the BAC by using the DIN roughness parameters: Rpk, Rk, Rvk, MR1 and MR2. I’m having a hard time making the calculation when I incur in non-isotropic roughness (that is when roughness is different in different directions)

My approximation of the area below the BAC is the following
Area Roughness, AR = Rpk * MR1 * 0.5 + (MR1 + MR2) * 0.5 * Rk + Rvk * (1-MR2) * 0.5 + Rvk * MR2

AR approximates the area under BAC with 3 triangles and one rectangle whose sides are given by Rpk, Rk, Rvk, MR1 and MR2. However, if you look at this approximation in a volumetric way, it too simplistically implies that the part has roughness Rk etc in one direction, and is 100% smooth in the other perpendicular direction. Though inadequate it has given me some limited success in predicting for how long I need to keep my part in a centrifugal tumbler (CBF).

Let say that I start from AR = 10 and I know that my media can at most give me a finish of AR = 6. If after 10 minutes I am at AR = 9, I can infer that I need another 10 minutes to reach AR 8 and, another 10 to reach AR = 7 and so on. But as I said above the part is not smooth in the perpendicular direction, and I need to combine the two ARs (no pun intended).

Any suggestion on how to calculate a geometric 3D equivalent of AR, let say a Volume Roughness VR?
 