Hello, I am trying to analyze a filler material, i.e. with a CTE of around 1E-4 1/F and modulus of around 500 psi. It is bonded in between two materials both with moduli greater than 1E5. The delta T of all three materials is around 150 F.
My question is, is there a general technique that allows this to be modeled accurately? When I equivalence the nodes, the large stiffness mismatch/CTE mismatch creates pretty unrealistic stresses. I then ran it with a glued contact solution (Patran sol 600) between the different materials which creates more realistic stresses than the equivalencing the nodes. Any thoughts on how to improve the fidelity of these analyses?
My question is, is there a general technique that allows this to be modeled accurately? When I equivalence the nodes, the large stiffness mismatch/CTE mismatch creates pretty unrealistic stresses. I then ran it with a glued contact solution (Patran sol 600) between the different materials which creates more realistic stresses than the equivalencing the nodes. Any thoughts on how to improve the fidelity of these analyses?