When welding a WT stiffener to the bottom of a W beam you get two different elastic section modulus: one for the top flange and one for the very bottom flange.
I am trying to stiffen a simply supported W beam with a yield strength of 240MPa with a WT with a yield strength of 350MPa.
Is it too conservative to use the lower 240MPa strength for the top flange or should I use a ratio of the yield strengths?
I am trying to stiffen a simply supported W beam with a yield strength of 240MPa with a WT with a yield strength of 350MPa.