Hello, I am developing a tool for obtaining forensic samples of powders from suspect surfaces. I would like to treat a porous substrate with a coating that will remain tacky after curing. This would allow adhesion of the particles for transport and analysis. Any ideas/suggestions are welcome. Thanks!