eeinpa
Electrical
- Nov 12, 2006
- 65
Hello. We've been trying to find a source for clutch and brake disks for a metal lathe which is no longer supported. We finally took it apart and measured the disks. We are thinking about just having new disks cut on a waterjet machine, as there really doesn't appear to be any rocket science to them. There is no friction material, just steel and steel disks. The disks are too thin for us to measure their hardness. Can anyone suggest a suitable steel to use to make these?
Thanks!
Thanks!