Aug 17, 2010 #1 SJKWS Petroleum Joined Jul 4, 2010 Messages 7 Location AU Looking for a good steel comparison chart from AS type steels to ASTM type to DIN/EN standards. eg AS1548- ASTM 516 - EN 10028.2 Regards SJKWS CWI
Looking for a good steel comparison chart from AS type steels to ASTM type to DIN/EN standards. eg AS1548- ASTM 516 - EN 10028.2 Regards SJKWS CWI
Sep 9, 2010 #2 bernoullies123 Mechanical Joined Dec 30, 2009 Messages 203 Location AU http://www.onesteel.com/images/db_images/productspecs/International Steel Grade Guide.pdf Upvote 0 Downvote
Sep 9, 2010 #3 isopvsw Mechanical Joined Jul 12, 2010 Messages 2 Location AU About the above link you get, be wary when you come acroos JIS 3101-55400, it's actually JIS 3101-SS400, AND also note that it's not Stainless Steel, but Structural Steel!!! Here is another one....mainly for Stainless Steels.... http://www.outokumpu.com/applications/documents/start.asp Upvote 0 Downvote
About the above link you get, be wary when you come acroos JIS 3101-55400, it's actually JIS 3101-SS400, AND also note that it's not Stainless Steel, but Structural Steel!!! Here is another one....mainly for Stainless Steels.... http://www.outokumpu.com/applications/documents/start.asp