The material that my state's spec book refers to for permanent steel sheet piling is AASHTO M202.

I can't seem to find this spec. without having to pay to download it. Does anyone know if this refers to a particular grade of steel? Also, I assume this is a corrosion resistant steel, although does this spec. include any particular coating?

Thanks for any help.
 
Replies continue below

Recommended for you

The ASTM spec is A328, F(tensile) = 65 ksi; F(yield) = 39 ksi.

It's a carbon steel. There is A690 marine grade sheeting.

Coating is something you have to discuss with the supplier.
 
You can now get sheets in ASTM A572 Grade 50 ksi, Which I think may be the most popular grade right now.
 