54
I am simulating a rolling process of steel. The model is 3D with symmetry planes in Y and Z directions. I am using Abaqus Explicit for this. The height reduction of the material is high - around 80%. The simulation runs successfully, however mesh elements deform heavily, so I want to use adaptive mesh. The problem is that when I turn on ALE adaptive mesh, the simulation terminates shortly after the beginning.

First, I will show you the case without adaptive meshing.
Before simulation:
2025_02_13-12_44_49.png

After simulation (elements are heavily distorted):
2025_02_13-12_47_49.png

So, I turned on ALE adaptive mesh:
2025_02_13-12_52_23.png

But the simulation terminates shortly after the start:
2025_02_13-13_09_35.png

The results for the last successful increment are given below:
2025_02_13-13_11_55.png

And the comparison between two simulations (with and without ALE adaptive meshing) at 0.015 step time (total time is 0.1):
2025_02_13-13_16_10.png

It can be seen, that the quality of mesh improved.
I don’t understand, why the simulation with ALE adaptive mesh terminates. Shouldn’t it be opposite?

Some bonus images with additional information:
2025_02_13-13_21_01.png
2025_02_13-13_22_07.png
2025_02_13-13_23_15.png

How can I solve this problem?
 

Attachments

  • 2025_02_13-13_21_01.png
    2025_02_13-13_21_01.png
    296.7 KB · Views: 4
Replies continue below

Recommended for you

Maybe try increasing the frequency of remeshing but also make sure that your loading is realistic - check the kinetic energy, perhaps mass scaling is too large.
 
The frequency is set to 1 per increment, so it can't be increased more:
2025_02_14-11_30_51.png

The kinetic energy is relatively low:2025_02_14-11_29_31.png
 
You could try playing with the ALE adaptive mesh controls. But the initial mesh (quality/shape of elements) also matters.

Check the documentation examples under Example Problems --> Static Stress/Displacement Analyses --> Forming analyses (especially "Flat rolling: transient and steady-state").
 