Can any one please tell me how to get the length of steel rebar specimen required to test the tensile strength according to ASTM A370. I cant get my hands on the code. therefore please help
 
Replies continue below

Recommended for you

Best to contact your testing lab to check what machine grips they use and the gauge length for elongation so you can then determine sample length.
 