Ok so i received these steel rebars today, but i am confused on the grade and strength of the bars, as you can see from the label, the bars are B450C according. to D.M. 14.01.2008 (Italy)
but then below you can see another 6 standards with different grades. so what is the yield strength of the steel bars i have in hand now? is it 450MPa or 500MPa?
this is their catalogue
this is their website
but then below you can see another 6 standards with different grades. so what is the yield strength of the steel bars i have in hand now? is it 450MPa or 500MPa?
this is their catalogue
this is their website