Not sure why you would need HCF data for this type of plate. The application for most high strength and toughness plates is typically for LCF service conditions, where you have thermal or pressure cycles (less than 10,000 cycles). I would suggest you contact ISG directly, or whomever now owns ISG, for HCF data. They may have performed such testing and did not publish it.