This is a typical flag pole type situation.

What is wrong with simply dropping a steel pipe in a hole and encasing it with concrete?? Don't worry about sizing of pipe or pier - that has been worked out. Structure is not for occupancy - literally a flagpole type application.

I assume that rust is the only real problem and if so - are there simple measures to prevent it.

Thanks for any help.
 
Is it a flagpole or something else? If it were a flagpole, there's nothing wrong with the concept per se. You still need to treat it as a drilled pier and would need to provide confinement reinforcement. If you need to replace the flagpole someday, it won't be easy to remove.
 
Three flag poles in a 60 x 60 x 70 triangle supporting a tent type canopy.

Good point on replacement --- but probably never happen.
 
I have done this for a numbe of projects from 3" square to 7 foot diameter, to support signs. As long as there is at least 3" of concrete cover, rust should not be a problem.

You can insert the poles into the wet concrete or pre-insert.

Another optin that cab be used for granular soils, the pole can actually be virated down to the required depth. Needs to be galvanised.

csd
 
Thats a thought --- I could pile drive it in....