Does anyone know where, preferably online, I can find physical properties for Low Carbon Steels at elevater temps such as 175 dC? I have looked on Matweb.

Thanks
 
Don't know about on-line, but thumbing thru the Metals Handbook, Vol I, most of the charts start at 370/400 dC. Don't think there is hardly any change up to 175dC.
 