Nov 26, 2003 #1 52447 Mechanical Joined Oct 25, 2003 Messages 2 Location CA Can anyone expound on the possibility of melting scrap baled steel sheets with an induction furnace and directly cast into 4mm x 100 strip to be subsequently hot rolled into 1.5 mm strips
Can anyone expound on the possibility of melting scrap baled steel sheets with an induction furnace and directly cast into 4mm x 100 strip to be subsequently hot rolled into 1.5 mm strips