Hello All,
I would like to ask your knowledge to get proposal for steel with these properties:
- yield strenght min 400 MPa
- tensile strenght min 500 MP
- elongation min 20%
- CVN-60°C min 20J
- CEV max 0,50 or max 0,60
- it should be for castings with wall thickness 50-100 mm
- it should be done without LF or VD(VOD) - only EAF or induction furnace
- heat treatment N, N+T or Q+T
I found out G14NiCrMo10-6 (1.6779, SEW685) but CEV is quite high. Russian steel 08G2DNFL(GOST21357) would pass perfectly but there is addition of yttrium or cerium and I dont know how to get it inside steel.
Any idea?
Dalin
I would like to ask your knowledge to get proposal for steel with these properties:
- yield strenght min 400 MPa
- tensile strenght min 500 MP
- elongation min 20%
- CVN-60°C min 20J
- CEV max 0,50 or max 0,60
- it should be for castings with wall thickness 50-100 mm
- it should be done without LF or VD(VOD) - only EAF or induction furnace
- heat treatment N, N+T or Q+T
I found out G14NiCrMo10-6 (1.6779, SEW685) but CEV is quite high. Russian steel 08G2DNFL(GOST21357) would pass perfectly but there is addition of yttrium or cerium and I dont know how to get it inside steel.
Any idea?
Dalin